technology
Lithium-metal anodes and dendrites
Also known as lithium metal anode, Li-metal anode, lithium metal batteries, LMB, anode-free batteries
A lithium-metal anode replaces a battery's graphite with pure lithium, which holds about ten times as much charge per gram, but lithium tends to grow needle-like dendrites that can short a cell, and it loses some active lithium as it cycles.[1][2][3] Low efficiency, short cycle life and safety concerns have kept it out of wide use in rechargeable batteries, and US programmes such as Battery500 target it for cells of up to 500 Wh/kg.[3][4]
Key facts
Reading order: how electrochemistry works, then the solid-electrolyte interphase, then this page. solid-state-batteries and lithium-sulfur-batteries follow it in the course.
What it is
Today’s lithium-ion cells store lithium inside a graphite anode. A lithium-metal anode uses the metal itself. The attraction is capacity: lithium metal holds 3,860 milliampere-hours per gram, about ten times graphite, and has a very negative potential of about -3.04 to -3.05 volts against the standard hydrogen electrode.[1][5] In a lithium-metal battery, lithium is plated onto the anode while charging and stripped off while discharging.[6]
An old idea that failed once
The first commercial rechargeable lithium batteries, in the 1970s, used lithium-metal anodes. They were abandoned because of dendrite growth and safety problems.[7] Lithium-ion cells with graphite anodes followed, gaining safety at a significant cost in energy density.[8]
Why lithium metal is hard
- Dendrites. In carbonate electrolytes lithium typically deposits as needle-like dendrites, which can grow through the separator to the other electrode, causing a short circuit and a possible fire.[2] How dendrites nucleate and keep growing is still not fully understood. One hypothesis is that uneven current creates local “hot spots” where lithium deposits first.[9]
- No host. Graphite and silicon hold lithium inside a structure. Lithium metal has no host, so its relative volume change is virtually unlimited, compared with about 10% for graphite and 400% for silicon cited in one review. That puts heavy strain on the protective SEI film.[10]
- Lithium loss. Forming the SEI consumes lithium and electrolyte.[11] Lithium can also become “dead lithium”, cut off from the current collector so that it no longer stores charge.[12] Together these problems mean low Coulombic efficiency (the share of charge recovered each cycle), poor cycle life and safety concerns, which have prevented wide commercial use.[3]
Testing conditions matter as well. Research cells often contain excess lithium, which inflates their apparent cycling efficiency. Practical cells need a negative-to-positive capacity ratio close to 1:1.[13] The most extreme version is the “anode-free” design, in which a bare copper current collector replaces the lithium anode.[6]
What researchers are trying
- Electrolyte design. A 2015 Nature Communications study reported that a highly concentrated ether electrolyte let a lithium-lithium test cell cycle more than 6,000 times at high current without dendrite growth, with Coulombic efficiency up to 99.1%.[14]
- Solid electrolytes. Solid electrolytes remove flammable liquid and physically block dendrites, but they usually conduct ions less well than liquids, and nearly all are unstable against lithium metal.[15] This is the bet behind solid-state-batteries.
- Understanding the interphase. In 2021 PNNL reported that a Battery500 team led by Brookhaven National Laboratory had detected lithium hydride in the interphase on lithium metal, addressing a long debate.[16] Operando video microscopy and in situ NMR are used to watch dendrites form and to measure where lithium is lost.[17][18]
Stabilising lithium metal is also seen as a key step for lithium-sulfur-batteries and lithium-air batteries.[19]
Battery500 and where things stand
The US Battery500 Consortium was formed in 2016 and is led by Pacific Northwest National Laboratory (PNNL). It aims for cells of up to 500 watt-hours per kilogram that last 1,000 cycles and cost well below 100 dollars per kilowatt-hour.[4] It focuses on lithium metal paired with high-voltage oxide cathodes and with sulfur cathodes, and works on dendrites and interfacial reactions among other problems.[20]
In June 2021 PNNL reported a 350 Wh/kg lithium-metal pouch cell that kept 76% of its capacity after 600 cycles. The lab said the technology was not yet ready for use, noting that vehicle lithium-ion cells typically last at least 1,000 cycles.[21] Cycle life, efficiency and safety are the hurdles the research cited here names for lithium-metal anodes.[3]
This page covers the research science. Company claims about lithium-metal and solid-state products are covered on solid-state-batteries and in the readiness debate.
Read next
Next in the crash course
Lithium-sulfur batteries
Lithium-sulfur batteries pair lithium with cheap, abundant sulfur for high theoretical energy density. How they work, the polysulfide problem and progress.
More in Batteries and energy storage
Questions readers ask
Why not just use lithium metal as the anode?
Lithium metal holds about ten times as much charge per gram as graphite, but it grows dendrites that can pierce the separator and short the cell, and side reactions keep consuming lithium. The first commercial rechargeable lithium-metal cells of the 1970s were abandoned for these reasons.[1][2][7]
What is a lithium dendrite?
A lithium deposit, typically needle-like in carbonate electrolytes, that grows during charging. It can grow large enough to reach the other electrode and cause a short circuit and possible fire. How dendrites start and grow is still not fully understood.[2][9]
What is "dead lithium"?
Lithium that has lost electronic contact with the current collector, so it can no longer store or release charge.[12]
What is an anode-free battery?
A design in which the lithium-metal anode is replaced by a bare copper current collector; lithium from the cathode plates onto the copper during charging.[6]
Will solid electrolytes solve the dendrite problem?
They could help, because they remove flammable liquid and physically block dendrites. But they usually conduct ions less well than liquids, and nearly all are unstable against lithium metal.[15]
Sources
· 22 claims from 9 publishers
Each numbered claim is a statement we checked against the sources listed with it. Tap a number in the text to see its sources in place.
- [1]
Lithium metal has a specific capacity of 3,860 milliampere-hours per gram, about ten times that of graphite at roughly 370. confirmedas of 2026-11-22
- A Review of Solid Electrolyte Interphases on Lithium Metal Anode · Advanced Science (Wiley), via PMC · Primary source · 2015-11-17 · Introduction (Li metal 3860 mA h g-1; graphite 370 mA h g-1) (retrieved 2026-11-22)
- Noninvasive In Situ NMR Study of "Dead Lithium" Formation and Lithium Corrosion in Full-Cell Lithium Metal Batteries · Journal of the American Chemical Society, via PMC · Primary source · 2020-11-23 · Introduction (retrieved 2026-11-22)
- [2]
Lithium deposited in carbonate electrolytes typically forms needle-like dendrites, which can grow large enough to pierce the separator and reach the other electrode, causing a short circuit and a possible fire. confirmedas of 2026-11-22
- Scientific Background on the Nobel Prize in Chemistry 2019: Lithium-Ion Batteries · The Royal Swedish Academy of Sciences (nobelprize.org) · Primary source · 2019-10-09 · p. 6 (retrieved 2026-11-22)
- High rate and stable cycling of lithium metal anode · Nature Communications, via PMC · Primary source · 2015-02-20 · Results (retrieved 2026-11-22)
- [3]
Low Coulombic efficiency, poor cycle life and safety concerns have prevented wide commercial use of lithium-metal anodes in rechargeable batteries. confirmedas of 2026-11-22
- Dendrites and Pits: Untangling the Complex Behavior of Lithium Metal Anodes through Operando Video Microscopy · ACS Central Science, via PMC · Primary source · 2016-10-14 · Introduction (retrieved 2026-11-22)
- [4]
The Battery500 Consortium, formed in 2016 and led by Pacific Northwest National Laboratory (PNNL), aims for cells with up to 500 watt-hours per kilogram, 1,000 charge-discharge cycles and a cost well below 100 dollars per kilowatt-hour. confirmedas of 2026-11-22
- Battery500 Consortium · Pacific Northwest National Laboratory · Primary source (retrieved 2026-11-22)
- Battery500 Consortium · Pacific Northwest National Laboratory · Primary source (retrieved 2026-11-22)
- Longer-Lived Lithium-Metal Battery Marks Step Forward for Electric Vehicles · Pacific Northwest National Laboratory (news release) · Primary source · 2021-06-28 (retrieved 2026-11-22)
- [5]
Lithium has a very low standard reduction potential, about -3.04 to -3.05 volts against the standard hydrogen electrode (SHE), which suits it to high-voltage, high-energy cells. confirmedas of 2026-11-22
- Scientific Background on the Nobel Prize in Chemistry 2019: Lithium-Ion Batteries · The Royal Swedish Academy of Sciences (nobelprize.org) · Primary source · 2019-10-09 · p. 3, Lithium section (value given as -3.05 V vs SHE for the Li+/Li couple) (retrieved 2026-11-22)
- Noninvasive In Situ NMR Study of "Dead Lithium" Formation and Lithium Corrosion in Full-Cell Lithium Metal Batteries · Journal of the American Chemical Society, via PMC · Primary source · 2020-11-23 · Introduction (value given as -3.04 V vs the standard hydrogen electrode, SHE) (retrieved 2026-11-22)
- [6]
In an "anode-free" design the lithium-metal anode is replaced by a bare copper current collector, and lithium plates onto it from the cathode during charging. confirmedas of 2026-11-22
- Noninvasive In Situ NMR Study of "Dead Lithium" Formation and Lithium Corrosion in Full-Cell Lithium Metal Batteries · Journal of the American Chemical Society, via PMC · Primary source · 2020-11-23 · Introduction (retrieved 2026-11-22)
- Noninvasive In Situ NMR Study of "Dead Lithium" Formation and Lithium Corrosion in Full-Cell Lithium Metal Batteries · Journal of the American Chemical Society, via PMC · Primary source · 2020-11-23 · Introduction (retrieved 2026-11-22)
- [7]
The first commercial rechargeable lithium batteries, in the 1970s, used lithium-metal anodes, but they were abandoned because of dendrite growth and safety problems. confirmedas of 2026-11-22
- A Review of Solid Electrolyte Interphases on Lithium Metal Anode · Advanced Science (Wiley), via PMC · Primary source · 2015-11-17 · Introduction (retrieved 2026-11-22)
- A reflection on lithium-ion battery cathode chemistry · Nature Communications, via PMC · Primary source · 2020-03-25 · The birth of rechargeable lithium batteries (retrieved 2026-11-22)
- [8]
Lithium-ion batteries with graphite anodes gained their safety at a significant cost in energy density compared with lithium metal. confirmedas of 2026-11-22
- A Review of Solid Electrolyte Interphases on Lithium Metal Anode · Advanced Science (Wiley), via PMC · Primary source · 2015-11-17 · Introduction (retrieved 2026-11-22)
- [9]
How dendrites nucleate and keep growing is still not fully understood; one hypothesis is that uneven current distribution creates local "hot spots" where lithium deposits first. confirmedas of 2026-11-22
- Dendrites and Pits: Untangling the Complex Behavior of Lithium Metal Anodes through Operando Video Microscopy · ACS Central Science, via PMC · Primary source · 2016-10-14 · Introduction (retrieved 2026-11-22)
- Dendrites and Pits: Untangling the Complex Behavior of Lithium Metal Anodes through Operando Video Microscopy · ACS Central Science, via PMC · Primary source · 2016-10-14 · Introduction (retrieved 2026-11-22)
- [10]
Lithium metal is a "hostless" anode, so its relative volume change during cycling is virtually unlimited, compared with about 10% for graphite and 400% for silicon cited in a 2015 review. confirmedas of 2026-11-22
- A Review of Solid Electrolyte Interphases on Lithium Metal Anode · Advanced Science (Wiley), via PMC · Primary source · 2015-11-17 · Introduction (graphite about 10%, silicon about 400%) (retrieved 2026-11-22)
- [11]
Forming the SEI consumes some anode material and electrolyte, lowering efficiency, but the layer also stops further direct contact between lithium and the solvent. confirmedas of 2026-11-22
- A Review of Solid Electrolyte Interphases on Lithium Metal Anode · Advanced Science (Wiley), via PMC · Primary source · 2015-11-17 · Introduction (retrieved 2026-11-22)
- [12]
"Dead lithium" is lithium that has lost electronic contact with the current collector, so it can no longer take part in cycling. confirmedas of 2026-11-22
- Noninvasive In Situ NMR Study of "Dead Lithium" Formation and Lithium Corrosion in Full-Cell Lithium Metal Batteries · Journal of the American Chemical Society, via PMC · Primary source · 2020-11-23 · Introduction (retrieved 2026-11-22)
- [13]
Research-scale lithium-metal cells often use excess lithium, which artificially inflates their apparent cycling efficiency; practical cells need close to a 1:1 ratio of negative to positive electrode capacity. confirmedas of 2026-11-22
- Noninvasive In Situ NMR Study of "Dead Lithium" Formation and Lithium Corrosion in Full-Cell Lithium Metal Batteries · Journal of the American Chemical Society, via PMC · Primary source · 2020-11-23 · Introduction (retrieved 2026-11-22)
- Noninvasive In Situ NMR Study of "Dead Lithium" Formation and Lithium Corrosion in Full-Cell Lithium Metal Batteries · Journal of the American Chemical Society, via PMC · Primary source · 2020-11-23 · Introduction (retrieved 2026-11-22)
- [14]
A 2015 Nature Communications study reported that a highly concentrated ether electrolyte (4 M LiFSI in dimethoxyethane) let a lithium-lithium cell cycle more than 6,000 times at 10 mA/cm2 without dendrite growth, with Coulombic efficiency up to 99.1%. confirmedas of 2026-11-22
- High rate and stable cycling of lithium metal anode · Nature Communications, via PMC · Primary source · 2015-02-20 · Abstract (retrieved 2026-11-22)
- High rate and stable cycling of lithium metal anode · Nature Communications, via PMC · Primary source · 2015-02-20 · Abstract (lithium|lithium cell at 10 mA cm-2) (retrieved 2026-11-22)
- [15]
Solid electrolytes could make lithium-metal cells safer by removing flammable liquids and physically blocking dendrites, but they usually conduct ions less well than liquids and nearly all are unstable against lithium metal. confirmedas of 2026-11-22
- Operando X-ray photoelectron spectroscopy of solid electrolyte interphase formation and evolution in Li2S-P2S5 solid-state electrolytes · Nature Communications, via PMC · Primary source · 2018-06-27 · Introduction (retrieved 2026-11-22)
- [16]
PNNL reported in 2021 that a Battery500 team led by Brookhaven National Laboratory had detected lithium hydride (LiH) in the interphase on lithium-metal anodes, addressing a long debate over whether LiH or lithium fluoride (LiF) forms there. reportedas of 2026-11-22
- Shining a Light Source on Batteries · Pacific Northwest National Laboratory (feature) · Primary source · 2021-01-28 (retrieved 2026-11-22)
- Shining a Light Source on Batteries · Pacific Northwest National Laboratory (feature) · Primary source · 2021-01-28 (retrieved 2026-11-22)
- [17]
Researchers have built visualisation cells to film lithium-metal electrodes during cycling (operando video microscopy) and match changes in surface shape, such as dendrites and pits, to the cell's voltage. confirmedas of 2026-11-22
- Dendrites and Pits: Untangling the Complex Behavior of Lithium Metal Anodes through Operando Video Microscopy · ACS Central Science, via PMC · Primary source · 2016-10-14 · Abstract (retrieved 2026-11-22)
- [18]
In situ nuclear magnetic resonance (NMR) has been used to measure where lithium is lost in a working anode-free cell, separating dead lithium from corrosion. confirmedas of 2026-11-22
- Noninvasive In Situ NMR Study of "Dead Lithium" Formation and Lithium Corrosion in Full-Cell Lithium Metal Batteries · Journal of the American Chemical Society, via PMC · Primary source · 2020-11-23 · Introduction (retrieved 2026-11-22)
- [19]
Stabilising lithium metal is also seen as a key step for lithium-sulfur and lithium-air batteries. confirmedas of 2026-11-22
- Dendrites and Pits: Untangling the Complex Behavior of Lithium Metal Anodes through Operando Video Microscopy · ACS Central Science, via PMC · Primary source · 2016-10-14 · Introduction (names Li-S and Li-air batteries) (retrieved 2026-11-22)
- [20]
Battery500 focuses on two chemistries, lithium-metal anodes with high-voltage, high-capacity metal oxide cathodes and lithium metal with sulfur cathodes, and works on dendrite formation and unwanted interfacial reactions among other problems. confirmedas of 2026-11-22
- Battery500 Consortium · Pacific Northwest National Laboratory · Primary source (retrieved 2026-11-22)
- Battery500 Consortium · Pacific Northwest National Laboratory · Primary source (retrieved 2026-11-22)
- [21]
PNNL reported in June 2021 that its Battery500 team had built a 350 Wh/kg lithium-metal pouch cell that kept 76% of its capacity after 600 cycles, while noting the technology was not yet ready for use and that vehicle lithium-ion cells typically last at least 1,000 cycles. reportedas of 2026-11-22
- Longer-Lived Lithium-Metal Battery Marks Step Forward for Electric Vehicles · Pacific Northwest National Laboratory (news release) · Primary source · 2021-06-28 (retrieved 2026-11-22)
- Longer-Lived Lithium-Metal Battery Marks Step Forward for Electric Vehicles · Pacific Northwest National Laboratory (news release) · Primary source · 2021-06-28 (retrieved 2026-11-22)
- Longer-Lived Lithium-Metal Battery Marks Step Forward for Electric Vehicles · Pacific Northwest National Laboratory (news release) · Primary source · 2021-06-28 (retrieved 2026-11-22)
- Longer-Lived Lithium-Metal Battery Marks Step Forward for Electric Vehicles · Pacific Northwest National Laboratory (news release) · Primary source · 2021-06-28 (retrieved 2026-11-22)
- [22]
Silicon plays a growing role as an anode component in lithium-ion batteries and is being explored for solid-state batteries, where it alloys at about 0.3 volts against lithium and so avoids lithium-metal plating and dendrites. confirmedas of 2026-11-22
- Chemo-mechanical failure mechanisms of the silicon anode in solid-state batteries · Nature Materials, via PMC · Primary source · 2024-01-26 · Main text (retrieved 2026-11-22)
- Chemo-mechanical failure mechanisms of the silicon anode in solid-state batteries · Nature Materials, via PMC · Primary source · 2024-01-26 · Main text (alloying at E = 0.3 V versus Li+/Li) (retrieved 2026-11-22)
Revision history (1)
- Page created.
Created Nov 22, 2026. Last reviewed by an editor on Nov 22, 2026. Next scheduled review: May 31, 2027.
Cite this page
"Lithium-metal anodes and dendrites." ContentLora, updated Nov 22, 2026. https://contentlora.com/wiki/lithium-metal-anodes